TECHNET Archives

December 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Pete <[log in to unmask]>
Date:
Thu, 15 Dec 2011 16:16:06 -0500
Reply-To:
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Type:
text/plain; charset="UTF-8"
In-Reply-To:
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (45 lines)
Pete,

 I have found the paste aperture adjustment logic in PCB design software rather poor. Such tools will under and over size well but when it comes to QFN thermal processing or home plate designs for passives these tools are totally lacking. I use PADs and Altium here.

 I would suggest folks generate 1:1  paste to pad apertures from the CAD tools and then provide rules to the stencil processor. The rules defined need to be coordinated with the stencil fabricator capabilities and hopefully the data exchange can be done electronically.

 I would be curious what PCB design tools you are using and how you adjust paste aperture using that tool. I am sure there are new tricks and capabilities I am not aware of.

Thanks,
Bob K.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete
Sent: Thursday, December 15, 2011 10:40 AM
To: [log in to unmask]
Subject: Re: [TN] BGA SMD vs NSMD

Most CAD systems allow you to adjust the soldermask aperture over (or under) size at CAM output.  This lets you change based on the design.  Some designs force you to use a smaller oversize, meaning you need to pay more for a fabricator that can do that for you.  Other designs have more room, you can use a larger opening, and a less expensive fabricator.

Again, I wouldn't recomend adding soldermask apertures to the CAD library.  There's a reason the CAD systems allow you to define them on the fly.

IPC-7351 really is a great "best case scenario" document.  But we rarely get to work in a "best case" world.

And don't let your fabricator change your artwork!  They have to make some process adjustments, but the final result in copper should match the gerbers you gave them.  Give them an inch........

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2