TECHNET Archives

October 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Croslin, Robert" <[log in to unmask]>
Date:
Fri, 11 Oct 2002 09:38:15 -0400
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Croslin, Robert" <[log in to unmask]>
Parts/Attachments:
text/plain (134 lines)
He must have one of them thee-raur-a-sus's.  They don't let us have them in
the south

Bob

 -----Original Message-----
From:   [log in to unmask] [mailto:[log in to unmask]]
Sent:   Friday, October 11, 2002 8:25 AM
To:     [log in to unmask]
Subject:        Re: [TN] no clean flux as a board cleaner?

I just love reading Brian's comments.  Where else are you going to find
someone use the word "horripilated"?

Doug





Brian Ellis <[log in to unmask]>@ipc.org> on 10/11/2002 03:16:26 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
       to Brian Ellis <[log in to unmask]>

Sent by:    TechNet <[log in to unmask]>


To:    [log in to unmask]
cc:

Subject:    Re: [TN] no clean flux as a board cleaner?


Genny

It's a long time since I heard such a suggestion :-( This is murder to
any reliability. Horrendous, horrent, horrible, horrid, horrific,
horrified, horripilated, horror-struck hardly describes it. NO WAY!

Brian

Genny Gibbard wrote:
> Consider a hand rework situation.
> We had a revelation from our production floor that occasionally a
> certain product is cleaned using a no-clean flux pen.  We have a product
> that the customer is very stringent that if we use no-clean solder on
> their product, we must not clean any residue off the board with our
> standard board wash.
> However, if a component is removed and replaced during a rework
> situation, often there is a lot of excess flux residue left on the
> board.  It came to light that in order to make this look better, they
> were applying a small amount of no-clean flux to the area with a flux
> pen, and then scrubbing the area with a brush.
>
> There were several horrified expressions around the table when this came
> to light.
>
> What would be the dangers of doing this?  The board is not heated like a
> reflow situation, or anything like that, after the 'cleaning' operation,
> so does this mean the flux may not be 'inert'?  I thought that it is
> no-clean flux used in the rework in the first place - why do they need
> to clean it off?  They said that it looked awful, and the inspectors
> wouldn't let the product thru if it wasn't cleaned up.
>
> Thoughts, suggestions?  Should we be horrified, or just let them
continue?
>
> Genny Gibbard (mailto:[log in to unmask])
>
>
----------------------------------------------------------------------------
-----

> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
>
----------------------------------------------------------------------------
-----

>

----------------------------------------------------------------------------
-----

Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2