TECHNET Archives

January 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Lum Wee Mei <[log in to unmask]>
Date:
Fri, 13 Jan 2012 07:30:38 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (87 lines)
Hi Wee Mei - one mistake in my last email - the X-ray gauge is a
Penetrameter and not a penetrometer.

Dave



Lum Wee Mei <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/13/2012 01:29 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Lum Wee Mei     <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
[TN] BGA X-ray baseline setting






Dear TechNet Buddies,

In IPC-A-600, the standard provides states the inspection magnification
requirement. For external observation : at 1.75x and progress to 40x if
acceptable condition of a suspected defect is not apparent. Such
inspection magnification requirement is not given in IPC-7095 for BGA
x-ray. What is the common industry practice on :

(a)    Tube voltage

(b)   Tube power

(c)    Filter strength

(d)   Averaging

I asked because I worry that I may unintentional set a 'wrong' tube
voltage that could result in the effect known as "Voltage Blooming'. I do
not want to cause false alarm due to my incompetency and result in wrong
inspection judgment on the void size.

Thanks and regards,
~wee mei~


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2