TECHNET Archives

October 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 4 Oct 2012 19:16:38 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Message-ID:
Subject:
From:
"Wenger, George M." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (76 lines)
Bob,

I assume that there must have been some sites where the solder on the pad had wet, or at least partially wet, the BGA solder ball otherwise it would have  fallen off instead of having to be pulled off.  Besides insufficient wetting could there also have been a Head-On-Pillow issue?

Regards,
George
George M. Wenger
Senior Principal Reliability / FMA Engineer
Andrew Corporation - Wireless Network Solutions
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 Office (732) 309-8964 Mobile
E-mail: [log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Thursday, October 04, 2012 7:46 PM
To: [log in to unmask]
Subject: [TN] The Great Broken Via Mistery

Hi,

 

  The other week I had posted about broken vias on an expensive PCB with filled vias. 

 

Well, let me inform folks about what really happened.

 

1.       There were no bad vias. The profile used  was low, only 221C at one
measured spot. They used leaded paste and lead free BGAs. 



2.       After pulling a part they found nice shiny reflowed pads and nice
round BGA balls that had never contacted.



3.       Today they fluxed and reflowed a dead board and it came back to
life.



4.       The Altera reflow process guidelines (AN 353) had errors in the
reflow tables. The Altera "Engineer" confirmed the data was good.  



Now I don't know who started this Bad Via story but my guess is a CM how screwed up doing a profile. Better to point fingers towards the board house is my guess Their "Engineer" thought that if parts got to 250C they would stop working. So using leaded paste on lead free parts was a really smart move. 

 

This is a classic case of people using data they think is good and forget to think, ask and observe. 

 

Such a big world, so many problem to solve and so much hogwash in so many heads.

 

Bob K.



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2