Might I suggest you contact Smartsonic in CA.
web site is http://www.smartsonic.com
They have solution that will assist in cleaning and don't damage any SMT components.
Wade Oberle wrote:
> Dear TechNetters,
> I have a fairly simple problem that I am looking for advice on.
> We use no-clean solder paste. How do some of you clean mis-printed
> boards with no-clean paste? How do you insure you get all of the paste
> out of the vias? If it is a double side reflow board and the first side
> is already populated, how do you clean mis-prints on side two and insure
> that paste from vias underneath large QFPs is completely removed? If
> you use certain chemicals and/or ultrasonic agitation, are there
> specific SMT components that are damaged by the use of these techniques?
>
> Thanks in advance for your replys.
>
> Wade Oberle
> Sr. Mfg. Engineer
> Manutronics, Inc.
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
--
Regards,
David Muscat
MANAGER
CAD SERVICE BUREAU
Arqtek Design
///////////////////////////////////////////////////////////////////
"DESIGN WIZARDS OF AUSTRALIA" (tm)
"THE EMC DESIGN WIZARDS" (tm)
///////////////////////////////////////////////////////////////////
[log in to unmask]
http://www.arqtek.com (Coming Soon!)
ph +61-3-9521-8139
fax +61-3-9521-8130
mobile +61-419-244-466
!!!!THE WIZARDS OF OZ!!!!!
PRODUCTS & SERVICES:
LASER STENCILS.
NICKEL Electroformed STENCIL.
Smartsonic Ultrasonic Stencil Cleaners and Chemistry.
Learnsoft MultiMedia Training Software for Electronics Manufacturing.
PCB Design with Protel.
PCB Design With Zuken Redac Visula High Performance tools.
PCB Design Benchmarking.
Process/ Production Engineering Consultancy.
We Deliver Price, Performance, Quality and Service!
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|