Ladies and Gentlemen,
After assembly of a board, it was discovered at test that there was an error
in the fab board causing a signal short. The inner layer short was cut and
a jumper installed to repair. I request guidance regarding the allowable
length for a jumper. I believe the linear length of this one to be about 4
inches. Can the installation of a jumper on a board's surface cause EMI
problems?
George Carroll
SE&A
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|