TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 5 May 2009 17:43:05 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject:
MIME-Version:
1.0
content-transfer-encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Joyce Koo <[log in to unmask]>
Parts/Attachments:
text/plain (190 lines)
You mean all the stuff contain in the black ink characters on a white paper? 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Tue May 05 14:59:15 2009
Subject: Re: [TN] What does HIGH GRADE FR-4 mean?

Hi again Karen,

Here's a couple of links that gives some idea of what's in the white
paper:

http://www.globalsmt.net/content/view/1184/106/

http://www.trafalgar2.com/documents/Columns-Engelmaier/7.1-engelmaier_2p
gs.pdf

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Karen Tellefsen
Sent: Tuesday, May 05, 2009 1:32 PM
To: [log in to unmask]
Subject: Re: [TN] What does HIGH GRADE FR-4 mean?

Do you have a reference for Werner's paper?

Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069



 

             "Stadem, Richard

             D."

             <Richard.Stadem@G
To 
             D-AIS.COM>                [log in to unmask]

             Sent by: TechNet
cc 
             <[log in to unmask]>

 
Subject 
                                       Re: [TN] What does HIGH GRADE
FR-4  
             05/05/2009 01:39          mean?

             PM

 

 

             Please respond to

              TechNet E-Mail

                   Forum

             <[log in to unmask]>

             ; Please respond

                    to

             "Stadem, Richard

                    D."

             <Richard.Stadem@G

                D-AIS.COM>

 

 





Hello, Harris,
You are correct that the customer (or circuit interface design engineer)
should provide the specific slash sheet describing the desired laminate
properties from IPC 4101B, as well as a description of the surface
finish as specified in IPC 4552, 4553, etc. Werner Engelmaier has an
excellent White Paper that includes everything that should be on a given
PWB drawing.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Harris Dy
Sent: Tuesday, May 05, 2009 12:23 PM
To: [log in to unmask]
Subject: [TN] What does HIGH GRADE FR-4 mean?

Hi All,

Can anyone define High Grade FR-4?

I think it's a vague requirement that I see on customer drawing. Is this
something that should be obsolete now because today customer should
really provide the properties of the laminate that they want to use...
eg Tg, Td, Dk.

Can anyone shed some light?

Thanks,
Harris




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2