I bet it's solder splashes. Tiny solder balls are flying in reflow ovens .
We investigated several cases like that in the past for our customers.
Regards,
Vladimir Igoshev
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7
Scarborough, ON M1R 5G1
Phone: 647-495-8727
Cell: 416-899-1882
[log in to unmask]
www.sentec.ca
Original Message
From: Steve Gregory
Sent: Wednesday, July 30, 2014 8:03 AM
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: [TN] Spots on Gold
Morning John,
I have your second photo posted, it's here:
http://stevezeva.homestead.com/ring.jpg
This looks interesting!
Steve
On Tue, Jul 29, 2014 at 5:56 PM, <[log in to unmask]> wrote:
> Hi steve
>
> I managed to get to a good microscope this afternoon. Everyone of these
> spots looks like someone circled it* w*ith a magic marker.
>
> Would you mind posting one more pic for me.
>
> Thanks
>
> John Foster
>
>
>
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary
or otherwise private information. Any unauthorized use, reproduction,
dissemination, distribution or other disclosure of the contents of this
e-mail or its attachments is strictly prohibited. If you have received this
email in error, please notify the sender immediately and delete the
original.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|