Graham Naisbitt wrote:
>
> Hi TechNetters,
>
> I would appreciate if anyone can give me a contact at RayChem. We are trying
> to source some suitable Surface Insulation Resistance Test cable, and have
> been recommended to use their PIVD.
>
> If anyone has any other recommendations, please let me know.
>
> Our requirement is for a sheilded 34 way ribbon cable that does not leach
> contaminants such as chloride gases into the test environment.
>
> Graham Naisbitt
> ------------------------------------------------------------------------------
> ----
> [log in to unmask]          Concoat Ltd
> Tel: +44(0)1276691100           Alasan House, Albany Park
> Fax: +44(0)1276691227           Camberley GU15 2PL UK
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ##############################################################


I may have a contact there from my previous job.

They make really good encapsulants.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2