TECHNET Archives

July 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bob METCALF <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bob METCALF <[log in to unmask]>
Date:
Wed, 10 Jul 2013 08:39:54 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (60 lines)
Try baking the affected boards for at least 30 min at 150C. I suspect you 
are getting some water absorption in the solder mask filler and if this is 
the case the bake will eliminate the white. If you don't have an oven for 
baking try using a heat gun directly to the white spots, that could work 
as well.

Regards,

Bob Metcalf
Atotech Western Regional Manager

Cell 714-334-7667
E-Mail [log in to unmask] 

This e-mail and any attachments hereto are business documents of Atotech 
USA Inc. and may contain CONFIDENTIAL OR PROPRIETARY BUSINESS INFORMATION. 
Unauthorized disclosure and/or use of information contained in this email 
is prohibited. If you are not the intended recipient, you may not read, 
use, disseminate or copy this message or any other files transmitted with 
it. 



From:   prashant chopra <[log in to unmask]>
To:     <[log in to unmask]>
Date:   07/10/2013 08:07 AM
Subject:        [TN] Black solder mask having white patch -- need advice
Sent by:        TechNet <[log in to unmask]>



Hi Everyone,
 
We are using a black soldermask for one of our PWA. After the assembly and 
aqueous wash cleaning, we see a white patch on the bottom side. This patch 
is in small area and the top side is all clean. Again this is not 
happening on all the PWAs. I have attached a picture above for reference.
 
I need expert advice on what can be the issues either from the PWB 
fabricator end or during the assembly process which can cause this? We are 
using the black solder mask for first time and we do not have such issue 
with either green or grey solder mask.
 
Thanks in advance for your help.
 
rgds
Prashant

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2