TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 15 Jun 2005 10:17:47 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (66 lines)
Hey, have a heart. Your message arrived at 16.38, local time and you
expect us to download, read and comment before dinner is ready, not
forgetting I had some other things to do in the same timeframe, such as
gardening? Pleeze!

Brian

Stephen Gregory wrote:
> Mornin' Everyone!
>
> Yesterday I had one of our test technicians come to me and
> ask if I knew of any good reference articles about the pro's and
> cons of Lead-free solders.
>
> He's doing a assignment in his college class about manufacturing
> processes. I first went on my rant about how mis-guided this whole
> thing is, and then told him that I was sure I could find him some good
> references.
>
> I did a search and found one that I had never seen before, and after
> reading it, I think it's the best one I've read. Go to:
>
> http://www.cepelec.com/iso_album/leadfreehmiller.pdf
>
> It's 53-pages, and very, very good!
>
> Kind regards,
>
> -Steve Gregory-
> Senior Process Engineer
> LaBarge Incorporated
> Tulsa, Oklahoma
> (918) 459-2285
> (918) 459-2350 FAX
> __________________________________________________________________
> This message may contain information that is privileged and confidential to
> LaBarge, Inc.  It is for use only by the individual or entity named above.
> If you are not the intended recipient, you may not copy, use or deliver
> this message to anyone.  In such event, you should destroy the message and
> kindly notify the sender by reply e-mail.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

--
______________________________________________
Please note new e-mail address [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2