On 9 Apr 2015 at 13:27, Steve Gregory wrote:
> Hi All,
>
> I'm wondering if I'm the only who is getting slammed by salespeople who are
> pushing this new GC10 solder paste from Loctite?
>
> I know the proof is in the testing and qualifying, but they are making some
> pretty hefty claims about this paste, like you can leave it on the stencil
> for 3-days, or that you don't have to refrigerate it and it has a year
> shelf life.
OK, maybe this works fine, why not?
I had in earlier days long before lead-free a solder paste from
Alphametals (something with ... 390... RMA) which could be left open
for days. I made prototypes with this paste down to 0.65mm pitch. One
day dispensing or screen printing, next day manual pick and place,
next day reflow soldering, and yes, cleaning was mandatory, but the
results were perfect. And this paste was even fine 1 year after
expiration date and after 1/2 year out of the fridge... just stir
well and fine.... no black magic, but, maybe a bit harder to achieve
nowadays with lead-free.
Regards
Matthias
--
Matthias Mansfeld Elektronik * Printed Circuit Board Design and
Assembly
Neithardtstr. 3, D-85540 Haar, GERMANY
Phone: +49-89-4620 0937, Fax: +49-89-4620 0938
Internet: http://www.mansfeld-elektronik.de
OpenPGP: http://www.mansfeld-elektronik.de/gnupgkey/mansfeld.asc
Fingerprint: 6563 057D E6B8 9105 1CE4 18D0 4056 1F54 8B59 40EF
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|