Hi Tim - manganin is an alloy comprised of 86% copper, 12% manganese, and
2% nickel.
Dave Hillman
Rockwell Collins
[log in to unmask]
superflx <[log in to unmask]> on 07/07/98 08:01:17 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to superflx <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: David D Hillman/CedarRapids/Collins/Rockwell)
Subject: Re: [TN] Manganin wire
What is manganin's composition?
Tim Frigon wrote:
> Any information on soldering interconnections made of manganin wire? The
> application uses small (AWG30 or smaller) manganin wire for thermal
> conductivity reasons. Current thought is to use very active flux to tin
> the wires, throughly remove any residues, and then solder the
connections.
> Any experience out there along these lines? Types of flux or solder to
> use? Currently using conventional Sn63 solder. Appreciate any help.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|