TECHNET Archives

December 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Yuan-chia Joyce Koo <[log in to unmask]>
Date:
Fri, 16 Dec 2016 07:53:04 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman <[log in to unmask]>
Message-ID:
Subject:
From:
David Hillman <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (61 lines)
Hi Joyce - are we talking black pad or black oxide (sometimes described as
black tar)? I was describing the black tar discussions we have had in the
IPC committees. Black pad is well understood and published.

Dave

On Fri, Dec 16, 2016 at 7:43 AM, <[log in to unmask]> wrote:

> http://ieeexplore.ieee.org/document/1645469/
>
> > Hi Mike - the general consensus is that there is an issue with the nickel
> > plating layer. Not a ton of data in the published literature but a topic
> > that has been discussed a length in the IPC-JSTD-002/003 committees at
> > times.
> >
> > Dave Hillman
> > Rockwell Collins
> >
> > On Thu, Dec 15, 2016 at 7:53 PM, Lehmicke, Michael <
> > [log in to unmask]> wrote:
> >
> >> What is the root cause of Black Oxide issues in ENIG plating?
> >>
> >> Mike Lehmicke
> >> Project Engineer
> >> DSS Division
> >> Molex, LLC-Printed Circuit Solutions
> >> 22 Empire Drive
> >> St. Paul, MN 55103
> >> 651-846-7728
> >> [log in to unmask]<mailto:[log in to unmask]>
> >>
> >> [cid:[log in to unmask]][cid:image001.jpg@
> 01D2345A.6B111BB0]<
> >> http://www.molex.com/>
> >>
> >>
> >> ________________________________
> >>
> >>
> >>
> >> CONFIDENTIALITY NOTICE: This message (including any attachments) may
> >> contain Molex confidential information, protected by law. If this
> >> message
> >> is confidential, forwarding it to individuals, other than those with a
> >> need
> >> to know, without the permission of the sender, is prohibited.
> >>
> >> This message is also intended for a specific individual. If you are not
> >> the intended recipient, you should delete this message and are hereby
> >> notified that any disclosure, copying, or distribution of this message
> >> or
> >> taking of any action based upon it, is strictly prohibited.
> >>
> >> English | Chinese | Japanese
> >> www.molex.com/confidentiality.html
> >>
> >
>
>

ATOM RSS1 RSS2