Hi Randy:
This is an idea. Make a template slightly larger
than the area needed to be cleaned ( 5/8" ) and place it over the area.
Use a wide solder iron tip, that has been sharpened, to scrap off the
solder mask. It should be a very fast operation, maybe twenty seconds
per.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jeffrey Bush
Sent: Thursday, November 10, 2005 3:34 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Mask Removal
You can use laser and solder by hand - laser can/usually is costly for
this type of rework. Ask your fab house to repair for you by hand -
taking mask off a tooling land/hand tinning is not hard. There are also
some repair houses that will do this also.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Randy Bock Sr.
Sent: Thursday, November 10, 2005 2:53 PM
To: [log in to unmask]
Subject: [TN] Solder Mask Removal
Hey y'all,
We have several hundred boards that are supposed to have the solder
mask
removed for around a mounting hole on the back side of the board. The
fab house missed. We are faced with a total remake if I cannot find
some way to remove the solder mask relatively easy. Most are still fab
boards, but I do have some that are assembled.
Any ideas would be appreciated. The clear area has to be approx 1/2 "
dia. (is for grounding)
Randy Bock Sr.
Quality Engineer
Pitney Bowes
AddressRight Printers
(email) [log in to unmask]
Newtown Building 2
203 270-4931 Ext
8-426-4931 In
203 270-4982 Fax
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|