Michael:
The fixture company in which we use is allowing us to use .025" test pads on
our up and coming PCB. Approx. 675 test pads. There is an additional
fixture cost for their custom "guided probe plate". This will be our first
fixture with .025" test pads. They tell me there will be no problems
probing these test pads.
Regards, Chris Bartkowiak
Acu-Rite Inc
-----Original Message-----
From: Michael Forrester [SMTP:[log in to unmask]]
Sent: Monday, July 16, 2001 9:14 AM
To: [log in to unmask]
Subject: [TN] ICT Test Points
Does anyone have any statistics on ICT reliability based on test
point size?
What I am looking for
is information on what am I giving up, other than cost, by going
from a .035
test pad to a .025 test pad.
Is there a reliability curve based on test point size? Any help
would be
appreciated. Thank you.
Best Regards,
Michael Forrester
LeCroy Corp.
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|