TECHNET Archives

February 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Ed Holton <[log in to unmask]>
Date:
Wed, 25 Feb 1998 09:21:20 -0400
Content-type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (30 lines)
When using an OSP coating on a double sided circuit board (plated thru),
should the topside annular ring of a via (not the area over the hole) be
covered with soldermask?  I am told by the designer that this is done to
prevent the copper from corroding during the lifetime of the product (no
conformal coat used).  Is it acceptable to have the soldermask go to the
edge of the via hole(over the annular ring) and allow some of the mask to
coat the upper portion inside the via hole.  I am having ICT failures on
probes that probe the bottomside of the via hole. Soldermask either covers
the via hole or bleeds down into the via hole, and then particles of this
soldermask are trapped in the solder "fillet" on the bottom of the board
that fills the via after the wave soldering process, and the probe does not
make contact.

Thanks

Ed Holton
Hella Electronics

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2