Couple comments on Russ Smith's posting:
1. I too heard that older laminate had a greenish hue, as the epoxy adhesion
promoter on the early glass fabric gave laminate a green tint (seems it was
chrome based, not silane?). Seems that 30 years ago, I remember the term
G-10, and not all was FR-4.
2. Slight correction on the pigments - blue is the color of non-halogen
phthalocyanine pigment, and green is the color when nearly fully chlorinated.
Think that is still the predominant blue/green pigment in many applications
- paints, inks, solder mask, etc. I have even heard that the environmentally
friendly Japanese symbol is a "blue leaf" symbolizing "green" ingredient
content. However, I have no confirmation. Russ, just a curious aside - Ciba
bought the DuPont blue/green pigment plant from DuPont in Delaware. It may
not have come into the Vantico fold, however.
Denny Fritz
MacDermid
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|