TECHNET Archives

June 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Ingemar Hernefjord (EMW)" <[log in to unmask]>
Date:
Wed, 19 Jun 2002 14:04:23 +0200
MIME-Version:
1.0
X-To:
Grant Emandien <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Ingemar Hernefjord (EMW)" <[log in to unmask]>
Parts/Attachments:
text/plain (69 lines)
Grant,

contact Sandra Winkler at :

Sandra Winkler is senior analyst at Electronic Trend Publications, San Jose, CA, (408) 369-7000, e-mail: [log in to unmask] Bance Hom is well known in the industry as the leading authority on IC Plating and is with Consultech International Inc., e-mail: [log in to unmask]

She has written a very good article with lots of refs in HDIonline. Actually, she has fallen in love with matte tin...she will perhaps tell you directly.

Regards

Ingemar Hernefjord
Ericsson Microwave Systems


-----Original Message-----
From: Grant Emandien [mailto:[log in to unmask]]
Sent: den 19 juni 2002 12:07
To: [log in to unmask]
Subject: [TN] Immersion Tin


Members,

A PCB supplier has requested us to evaluate immersion tin as a finish.
Immediate concerns raised were shelf life, solderability, whiskers, etc.
Researching the archives has noted similar as well as opposing views and
concerns. In addition to possible problems arising from immersion tin
finish, what PCB fabricator process changes may contribute to possible
reliability and solderability concerns and how this impacts production
processes such as reflow. The proprietary chemistry used is MacStan HSR from
Macdermid.

Anyone willing to share experiences and guide me towards making an informed
decision.

TIA
Grant


**********************************************************************
Notice:

This email transmission contains confidential information which is the property of the sender. The information is intended only for the use of the addressee. If you are not the intended recipient, you are hereby notified that any disclosure, copying or distribution of the contents of this e-mail transmission, or the taking of any action in reliance thereon or pursuant thereto, is strictly prohibited. Should you have received this email in error, please immediately notify us by telephone to arrange for return of the documentation comprising this transmission. In no event will Tellumat (Pty) Ltd or the sender of this email be liable to any party for any direct, indirect, special or other consequential damages for any use of this email, or on any other hyper linked website, including, without limitation, any lost profits, business interruption, loss of programs or other data on your information handling system or otherwise, even if we are expressly advised of the possibility of!
 such damages.

**********************************************************************

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2