has anyone been successful with a via in pad that is not plugged? YES
If so, was it double sided? NO
And, was one side connected to a BGA ball? YES
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ryan Grant
Sent: Monday, February 04, 2008 4:55 PM
To: [log in to unmask]
Subject: [TN] Open via in pad - any success?
Hi All,
I just got told by a design engineer that LaserJet printers are built using
via in pad where the via is NOT plugged. He claims the via is filled with
solder first, then goes through the normal SMT process.
He intends to use this to connect a BGA ball on one side of the board to a
cap on the other side using an mechanically drill via that is not plugged.
Before I call BS on this, and tell him "do not pass go until that via is
plugged, flattened and plated over", has anyone been successful with a via
in pad that is not plugged?
If so, was it double sided?
And, was one side connected to a BGA ball?
Thanks,
Ryan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|