TECHNET Archives

August 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 7 Aug 2015 16:25:37 -0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ricardo Moncaglieri <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; charset="UTF-8"
From:
Ricardo Moncaglieri <[log in to unmask]>
Parts/Attachments:
text/plain (25 lines)
Estimated colleagues,
In some cases componentĀ“s thermal planes Au finished which will be
solded on ENEPIG TMM10 pcb where coplanarity is very critical then
pretining modify undesirably coplanarity.
Taking into account this fact, we have reflowed the component (solder
the earth plane to pcb) without pretining and compare soldering under RX
to another done with pretining. Have found out no difference between
both cases (with and without pretining).
Furthermore will run some tracking tests to verify joint.

My question:

Do you know or have any background experience on soldering Au finished
thermal planes without pretining?
In all other cases of Au components terminals finished, we always
remove Au.
 
brgds,Ricardo


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2