TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wGnG8-000BjKC; Mon, 14 Apr 97 10:01 CDT
Encoding:
42 Text
Old-Return-Path:
Date:
Mon, 14 Apr 97 10:09:20 cst
Precedence:
list
Resent-From:
Cc:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11931
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"wAGIh2.0.fpF.CRaKp"@ipc>
Subject:
From:
"ddhillma" <[log in to unmask]>
X-Loop:
From [log in to unmask] Mon Apr 14 15:
52:50 1997
Resent-Sender:
TechNet-request [log in to unmask]
Message-Id:
Parts/Attachments:
text/plain (55 lines)
     Hi TechNet!
     
     Try conducting a thermal profile of your board with a thermocouple 
     attached to the QFP pads and a thermocouple attached to the QFP leads 
     - you may have uneven heating with the board internal layers thieving 
     enough heat that the leads become the preferred direction for solder 
     flow. The thermal profile data should help point you in the right 
     direction. Good Luck.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: Reflowing gold plated board
Author:  [log in to unmask] at ccmgw1
Date:    4/12/97 12:54 PM


I am processing a board with pads that are gold plated. I am using OA 
paste 63/37. All the pads are flowing good except for a  QFP. Shorts are 
appearing after reflow. The screen apertures are the same dims that i 
normally use for HASL boards. The profile is set to the low side 
temperature wise ( i tried a higher temp and it was just as bad). It 
appears that the solder is not flowing evenly between the pads and the 
leads. It is flowing more so to the leads than the pads.  I also tried 
applying a liquid OA flux to the leads of the QFP prior to reflow and that 
made the shorts even worse. Anyone have any suggestions. Thanx
ahead.
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2