TECHNET Archives

December 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bev Christian <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Mon, 22 Dec 2008 20:15:37 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (108 lines)
That was supposed to be "to think". Too bad Spell Check doesn't check that sort of thing. 
Bev

----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Mon Dec 22 20:12:30 2008
Subject: Re: [TN] Underfill, inhibition due to leftover activators in the flux residue

Phil,
I have had more time outthink about this now.  A good chili on a winter
night helps.  :)

This could be really bad news. I have not heard of this before.  The good
news is that the joints most at risk during thermal cycling and drop are the
ones the farthest from the neutral point, which is where (neutral point) you
are finding the phenomenon.  Even so, I am concerned.  Now I am wondering
how many other combinations are doing this?
Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phillip Bavaro
Sent: Monday, December 22, 2008 6:02 PM
To: [log in to unmask]
Subject: [TN] Underfill, inhibition due to leftover activators in the flux
residue

I have made quite a few test samples and discovered that a certain 
underfill material will exhibit inhibited cure when it comes in contact 
with solderpaste flux residues at the center of a very dense BGA component.
The rest of the underfill beneath the BGA will harden like normal.
We don't clean nor plan on starting to clean our assemblies.
DVT testing does not show any defects due to underfill adhesion.


Background:
We used a four up ABAB panel which goes through SMT twice.
BGAs only passing through the oven once consistently show the problem.
Two passes through the reflow oven (ABAB flip) and the problem goes away.
This means that  half of our test samples still have soft material in the 
pocket at the center where the power ground pins are located.
We measure peak temperature in this area and have found that raising the 
peak temperature helps quite a bit but does not eliminate the inhibition 
entirely.
The manufacturers of the paste and the underfill acknowledge the issue but 
do not have a solution.

Has anyone else run into similar compatibility issues with a paste and 
underfill?

In the event that we cannot work out the root cause, and decide to make a 
change, I am trying to come up with a list of all the manufacturers of 
underfill.

So far I have found 8 major underfill manufacturers but would appreciate 
knowing about more if there are any.

3M
Ablestik
Epotek
Henkel
Hysol
SP&S
Sunstar
Zymet

Thanks in advance,

Phil

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2