Totally agree with Brian. In addition, use RTV around connector or
relay or any switch elements are trouble some. The RTV outgas and
migration of silicone will result intermittent and poor contact in the
long run. I thought it was not permit for such a usage many years ago.
Major reliability concerns! (check early 90, late 80s papers).
Scary! Hopefully, it is not on aircraft or anything moving....
jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
>Sent: Tuesday, March 18, 2003 11:47 AM
>To: [log in to unmask]
>Subject: Re: [TN] How to hold component in socket
>
>
>Genny
>
>For goodness sake, do NOT use an RTV that smells of acetic
>acid. Wanna know why? Because it emits acetic acid! And what
>does acetic acid do to electronics, in a semi-closed
>environment and under uncontrolled climatic conditions such as
>in transport? SHUDDER!
>
>Brian
>
>Genny Gibbard wrote:
>> Do any of you seem to work somewhere where RTV is the answer to
>> everything???
>>
>> We have a PCB with a DIMM socket. The DIMM is inserted at one angle
>> and then pushed down and 'locks' in at another angle to the PCB.
>> Problem is, the catch mechanism isn't very strong and sometimes the
>> DIMM pops back up to the insertion angle. We're concerned that when
>> we ship these cards, the DIMM will pop loose and eventually work its
>> way out of the socket. Any suggestions as to how to hold it
>in place?
>> We don't want to do it so permanently that we can't ever remove and
>> replace a defective DIMM. The suggestion around here is a dab of
>> silicone RTV...
>>
>> Genny
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a free service by IPC using LISTSERV
>> 1.8e To unsubscribe, send a message to [log in to unmask] with
>following
>> text in the BODY (NOT the subject field): SIGNOFF Technet To
>> temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives Please visit IPC web site
>> http://www.ipc.org/html/forum.htm for additional information, or
>> contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
>> -----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using
>LISTSERV 1.8e To unsubscribe, send a message to
>[log in to unmask] with following text in the BODY (NOT the
>subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
>mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest Search the archives of
>previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/html/forum.htm for
>additional information, or contact Keach Sasamori at
>[log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|