Hi,

 Yes, Gordon Davy wrote that and I was the person who formatted the text to
make it look nice, and I generated the .pdf file! It was such a good write
up I wanted to pass it along.

I think the cross section of a paper towel is mostly air, and water vapor
diffusion through the towel cross section should be quite high. I just don't
know the numbers.

 Yes that vacuum thing seems to be hog wash if I understand things
correctly. (Big If)

Bob K

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Tuesday, April 09, 2013 2:01 PM
To: [log in to unmask]
Subject: Re: [TN] Pakeout and PCB Separators

Someone in Technet not long ago posted up an excellent little write up from
Gordon Davy about water vapor and drying.  I've attached it to Phil and Bob.

It contends vacuum ovens do nothing to increase drying rate.

Drying is a function of temperature and delta between concentration of water
in the middle versus at the surface.   

I presume, like any drying, the greater the surface area exposed the faster
the drying.  I would place the PCBs (as much as possible) directly on racks
or in card holders (on edge).
 
-----Original Message-----
From: Nutting, Phil [mailto:[log in to unmask]]
Sent: Tuesday, April 09, 2013 1:01 PM
To: [log in to unmask]
Subject: Re: [TN] Pakeout and PCB Separators

Robert,

How about placing them in a vacuum chamber.  That would release all the
moisture and definitely if you could add a little heat.  I would envision
separating the boards with a mesh and spacer to allow the moisture to fully
escape.  Placing a paper towel between layers might not let all the moisture
escape.

But then this is just my opinion.

Phil Nutting

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Tuesday, April 09, 2013 12:54 PM
To: [log in to unmask]
Subject: [TN] Pakeout and PCB Separators

Hi,

 

Does anyone know if separators of some type between PCBs can reduce bake out
time?

 

If I have a stack of PCBs, and I place something like paper towels between
PCBs, can the bake out time be reduced? I would imagine the diffusion rates
of moisture in the paper towel material would be much higher than in solid
PCB laminate. But, that is just a guess. Could be perfect hog wash.

 

My problem is not with PCBs but with 30 mil sheets of plastic that feed a
thermoforming process.  I am using PETG but I still see small bubbles in the
material after forming. I tried a short bake out, and it helps, but I cannot
heat very high as the 30 mil plastic sheets will easily deform. I need to
lay them flat, heat gently, and still try to removed moisture. I was
wondering what the best way to separate sheets and allow drying might be.

 

Any Ideas?

 

Thanks,

Bob K.

 



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2