There seems to be a few values missing.
If we knew the board size, we'd be able to calculate the flux spray exposure time, from this we can determine volume of flux deposit in ml/sq. in.
If we knew the specific gravity of the flux, we could determine the weight of the solids per given volume, i.e., ug/ml.
Ed Popielarski
Engineering Manager
970 NE 21st Ct.
Oak Harbor, Wa. 98277
Ph: 360-675-1322
Fx: 206-624-0695
Cl: 949-581-6601
“It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design.”
https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kenny Munro
Sent: Wednesday, February 25, 2015 5:53 PM
To: [log in to unmask]
Subject: [TN] Wave Solder Flux Loading formula
I am looking for a formula to calculate the wave solder flux loading / deposition in - μg/in2 of solids or μg/cm2 of solids with the following machine parameters,
Flux solid content : %
Conveyor speed : m/min
Flux Spray Volume : ml / min
Spray Head Traverse : mm / sec
Does anyone know if there is a calculation that can be used to give the loading? Any help would be most appreciated.
Kenny Munro
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|