Andy:
The potential for this would depend on some specifics. However, generically depending on the mixture ratio
of tin/zinc one alloy that I have seen used was a 91Sn9Zn. This piticular mix has 14 deg. F higher melting
temperature and has (although I do not believe that you need it) a higher tinsel strength.
TBlack
Microwave Engineering
Andy Mackie wrote:
> Does anyone have any experience with tin/zinc alloys? I heard that Toshiba
> has done some work with these, and I'd love to know if it's a viable
> lead-free alternative for electronics assembly, and what the drawbacks are.
>
> Thanks!
>
> Andy Mackie, PhD (Chairman - IPC Solder Paste Task Group)
> Praxair Inc.
> 777 Old Saw Mill River Road
> Tarrytown
> NY 10591
> Ph: 914-345-6402
> Fx: 914-345-6405
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|