TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Kelly M. Schriver" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 18 Aug 1998 09:44:09 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (47 lines)
Dave - Tenting of vias is a wise precaution to reduce the potential for
intermetallic growth formations between exposed conductors.  The more exposed
metal you have under part bodies and in hard to clean areas, then the  greater
the risk that some small amount of process residue, coupled with moisture and
operating current, will become a problem.  Vias themselves can also represent
a cleaning problem, simply from their small size.

Even though solder mask is not to be used as a conformal coating, you will
note that its dielectric values and process durability are quite respectable
for this purpose.

A word of caution: some of the less durable solder masks are not necessarry
acceptable to tent vias.  The heat of soldering can generate considerable
pressure from the atmosphere in  a via, causing the mask tent to rupture.
Recommend you test this thoroughly, as ruptured via tents tend to inhale
process fluids as they cool following soldering.

As with any solder mask application, IPC-SM-840 indicates that the user must
confirm compatibility with his own processes and applications.  We have
encountered a number of masks which are susceptible to some of the non-CFC
cleaners, as well as a few which reacted to various fluxes.

Regards - Kelly

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2