TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Mcmaster, Michael" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 23 Apr 1999 08:14:56 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (54 lines)
Your proposed requirement is equivalent to the current IPC 6012 spec
(0.75%) for boards 6"x6"or smaller.  What would be your maximum board
size?  If 18"x24", .065 would be equivalent to 0.27% for bow and 0.21%
for twist.  I have a panel that size at my desk but no pin gages to
measure the deflection.  I also have a micrometer and paperclip that is
0.035" thick and it won't fit under the board anywhere so this board
would meet your spec.

A good design with balanced construction can probably be built to your
spec, but you can expect a lot of questions and even resistance when
people see your requirement.

If your designs are unbalanced, it can be difficult to meet the IPC
standard much less something more stringent.

> ----------
> From:         Richard Hamilton[SMTP:[log in to unmask]]
> Reply To:     TechNet E-Mail Forum.;[log in to unmask]
> Sent:         Wednesday, April 21, 1999 12:03 PM
> To:   [log in to unmask]
> Subject:      [TN] Bow and Twist
>
> Hello TechNetters,
>
> I really hate to beat an almost dead horse to death, but........
>
> I would like opinions on a requirement for Bow (Warp) and Twist that
> calls
> for .065" maximum on any size board. Is this unreasonable? Can it be
> done?
> Does it require more than normal handling? Does it require excessive
> extra
> handling?
>
> As usual, Thanks in advance for your assistance!
>
> Richard Hamilton
> Clemar Mfg. / Rain Bird
> [log in to unmask]
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2