Dear All,
Shall we follow the table 8.2 or the following requirements?
Figure 8-39 610D-08-030
Acceptable - Class 1
* Wetted fillet is evident.
Acceptable - Class 2
* End overlap (J) between the component termination
and the land is minimum 50% the length of
component termination (R).
Acceptable - Class 3
* End overlap (J) between the component termination
and the land is minimum of 75% the length of
component termination (R)
Thanks!
Regards
Geok Ang