Franklin D Asbell wrote:
>
> The board shop would only be at fault (partially) in this case if they
> failed to express the fact that immersion tin is a poor coating for
> press-fit connectors...the remaining fault would be the process or design
> personnel...
> snip <

        That's an interesting response, since we've had reputable
        fab vendors recommend IWT finish for pressfit.  Apparently
        it is easier to maintain tight hole size tolerances with
        this compared to HASL.

        What issue makes IWT a poor choice for pressfit, if you've
        got a good process with uniform results?  (personally, I'm
        more nervous about leaving IWT unpassivated (ie soldered)
        in long lived equipment due to possible whisker growth)

        TRhanks,
--

      Jeff Seeger                         Applied CAD Knowledge Inc
      Chief Technical Officer                  Tyngsboro, MA  01879
      jseeger "at" appliedcad "dot" com                978 649 9800

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2