Steve,
I cannot speak about anything able to survive total prolonged submersion in
nasty stuff like fuel but...
I can tell you that HumiSeal 1A33 polyurethane was successfully tested for
resistance against "Skydrol", a particularly nasty aggressive aviation
hydraulic fluid. You just need to bake the **** out of it to get the best
protective results!
I hope this might help
Regards,
Graham Naisbitt
[log in to unmask]
WEB: http://www.concoat.co.uk
CONCOAT Ltd
Alasan House, Albany Park
CAMBERLEY GU15 2PL UK
Tel: +44 (0) 1276 691100 Fax: +44 (0) 1276 691227
----- Original Message -----
From: Stephen R. Gregory <[log in to unmask]>
To: <[log in to unmask]>
Sent: 11 October 1999 13:50
Subject: [TN] Fuel resistant laminate...
> Mornin' everybody!
>
> Well, here I am at the ol' salt mine. Thanks to everybody who replied to
my
> "blowin' off some steam" email. There was a lot of good advice. I would
like
> to be able to sit down make some "whiz-bang" presentations to convince
> certain people about changing things, but the fact of the matter is, I
flat
> don't have the time. Too busy fighting fires...but I really don't want to
get
> into all that again.
>
> Anyway, I was asking again if there's any recommendations for a good
laminate
> material to use that will withstand fuels, and a coating to use to cover
the
> electronics on it. I've got my Clyde F. Coombs Jr. book and will be
pouring
> through the pages.
>
> This is supposed to be used for a fuel quantity indicating system...
>
> Thanks! Try and have a great Monday guys, I'm gonna...
>
> -Steve Gregory-
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|