TECHNET Archives

August 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 28 Aug 2001 11:52:26 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (42 lines)
I come again to the collective Delphi Oracle!

I have the job of specifying to PCB fabricators what we want them to build,
even though I have no previous direct experience in doing this. I'm trying
to have a 12 layer board fabricated that is VME standard - 0.063+/-0.008"
thick. It contains 6 x 1 oz copper signal layers and 6 x 2 oz plane layers
in the stack-up 1-2-2-1-2-1-1-2-1-2-2-1. To maintain the 0.063" thickness,
I have called for 3.5 mil thick Core and Pre-preg in accordance with the
minimum requirements of MIL-PRF-55110 (I know this is being superceded by
IPC-A-6012, BTW).

The feedback I'm getting is that the dielectric spacing between adjacent 2
oz layers in particular is far too thin and should be 8 or 10 mils of
pre-preg. Even between 1 oz copper layers, the recommendation is for 5
mils. I can't seem to get a quick and clear explanation as to WHY the fab
house is recommending these thicknesses.

My question is: does the pre-preg thickness have to take into account the
bordering copper weights in addition to the minimum dielectric spacing?
i.e. for adjacent 2 oz copper planes, should my pre-preg thickness spec be
2.8+3.5+2.8 = 9.1 mils? What is the "formula"?

Sorry for such a basic question, and my TIA for the help I feel sure I'll
get.

Pete Duncan

[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2