TECHNET Archives

April 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Ofer Cohen <[log in to unmask]>
Date:
Wed, 30 Apr 2003 10:42:59 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Franklin D Asbell <[log in to unmask]>
Parts/Attachments:
text/plain (70 lines)
The board shop would only be at fault (partially) in this case if they
failed to express the fact that immersion tin is a poor coating for
press-fit connectors...the remaining fault would be the process or design
personnel...

HASL is by far a better coating for use in press fit connectors...as you've
noticed from the exposed copper...and yes, the hole wall will look pretty
cra**y...

This is one of those (DOH!!! we did not think this assembly process through
well enough) situations

Franklin


----- Original Message -----
From: "Ofer Cohen" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, April 30, 2003 9:47 AM
Subject: [TN] External finish selection


> Techneters,
> The back planes of our products include many press fit connectors (1200 to
> 6000 pins) and 100 to 500 passive components - resistors and capacitors,
> mostly 0603 and 0402. In the past we used HASL finish. However, during the
> last year we switched into immersion tin. Following some failures in the
> coating processes, yielding exposed copper on external pads (and you can
> just imagine what happens in the via and connectors pins holes), I
consider
> two options:
> 1.      Replace my old and known vendor, and look for one who will do a
> great job in the coating, or
> 2.      Return to the good, old, well known and reliable HASL.
>
> I think that my tendency can be read between (or inside) my lines; yet, as
I
> have not made my final decision, I am open for other opinions.
>
> Regards
> Ofer Cohen
> Quality Assurance Manager
> Seabridge Ltd.
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2