TECHNET Archives

July 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Date:
Wed, 22 Jul 2009 22:38:28 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
From:
Parts/Attachments:
text/plain (100 lines)
Don't, Rudy.
Read Epson's new policy in the IBM report I recommended: a CLEANER 
ENVIRONMENT.
Maybe this will be a corner stone in the US future marketing! Your country 
may be the leader, don't strangle the baby.
/Inge

----- Original Message ----- 
From: "R Sedlak" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, July 22, 2009 10:24 PM
Subject: Re: [TN] DOP in ESD flooring


With the caveat that free advice is often not worth what you paid for it...

DOP and ESD have zero to do with each other, DOP MAY have a health concern, 
but frankly, given the high level of ventilation in most facilities, even if 
it has some effect, I would not concern myself. DOP will out-gas, if very 
slowly. This is often what you wipe off the interior of your windshield in 
your newer car.

Rudy Sedlak
RD Chemical Company
--- On Wed, 7/22/09, Bruce Tostevin <[log in to unmask]> wrote:

From: Bruce Tostevin <[log in to unmask]>
Subject: [TN] DOP in ESD flooring
To: [log in to unmask]
Date: Wednesday, July 22, 2009, 12:40 PM

Hi All,

We're preparing to install thousands of square feet of ESD flooring in a
new manufacturing space and have different vendors talking to us about
tiles which are, or are not - DOP FREE. A quick search tells us that
DOP is Dioctyl phthalate, a widely used plasticizer used in everything
from plastic buckets to foods.

Questions:

How great a consideration is it that ESD flooring has or does not have
DOP additives?

Is it a long term health concern, subject to any outgassing, leaching,
etc.

Does DOP improve the ESD qualities or longevity of the flooring compared
to flooring that does not contain it?

Any help would be much appreciated,

Thank you,

Bruce Tostevin
Benchmark Electronics
Hudson, New Hampshire

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------





---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2