That looks much better, because at our company, which is rather big, we use
a lot of ENIG.
Inge
----- Original Message -----
From: "Dennis Fritz" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, September 19, 2006 8:51 PM
Subject: Re: [TN] ENIG - surface finish chemistry revenue
In a message dated 9/19/2006 10:48:10 A.M. Eastern Daylight Time,
[log in to unmask] writes:
Thanks Denny! A few of us were questioning that the data was so old,
crust was forming, which is appropriate for a pie chart. Let us know if
you get any updates.
Dewey
Dewey,
I only have the year end 2003 data at hand today. And, remember how the
Suppliers Council tracks this data - by the revenue from the chemistry - not
by
the square feet of boards. So you have to use some multiplier or factor to
estimate square feet of boards, but this is not too bad as it leaves the
metals (gold) value out of ENIG.
Here were the percent of chemistry sold for finishes in the US in 2003:
HASL- 22.4% (I can't tell if this includes the metal added to the solder
pot
- doubt it)
OSP – 34.3%
ENIG – 15.0% without metal content (gold)
Imm Sn – 7.1%
Imm Ag – 13.6%
Other metallics – 7.5%, presume this is electroplated nickel gold or
reflowed tin lead.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|