TECHNET Archives

March 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Paul Wilson <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 3 Mar 1999 06:18:12 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (57 lines)
Howard,

It might be that the reverse order of application would be acceptable for a wire bond?
Is this an "all gold board"?
The tab plater would likely sheer the immersion gold off anyway?

                        Paul Wilson
        R&D Manager / Plant Chemist

                   Circuit Center, Inc.
                 4738 Gateway Circle
                  Dayton, OH 45440

          Phone (937) 435-2131     Fax (937) 435-7698
            http://www.circuitcenter.com

-----Original Message-----
From:   Howard Lin [SMTP:[log in to unmask]]
Sent:   Wednesday, March 03, 1999 12:07 AM
To:     [log in to unmask]
Subject:        [TN] Two kinds of surface finish

Dear All,
I got one inquiry from our customer on two kinds of surface finisf for
one board. They need both immersion gold and hard gold plating. Can I
dirctly apply hard gold plating over immersion gold on gold finger area?
Is there any quality issue that I should concern?
I am very appreciated  for any input.
Regards,

Howard
Maxedge Electronic Corp.
[log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2