Howard,
It might be that the reverse order of application would be acceptable for a wire bond?
Is this an "all gold board"?
The tab plater would likely sheer the immersion gold off anyway?
Paul Wilson
R&D Manager / Plant Chemist
Circuit Center, Inc.
4738 Gateway Circle
Dayton, OH 45440
Phone (937) 435-2131 Fax (937) 435-7698
http://www.circuitcenter.com
-----Original Message-----
From: Howard Lin [SMTP:[log in to unmask]]
Sent: Wednesday, March 03, 1999 12:07 AM
To: [log in to unmask]
Subject: [TN] Two kinds of surface finish
Dear All,
I got one inquiry from our customer on two kinds of surface finisf for
one board. They need both immersion gold and hard gold plating. Can I
dirctly apply hard gold plating over immersion gold on gold finger area?
Is there any quality issue that I should concern?
I am very appreciated for any input.
Regards,
Howard
Maxedge Electronic Corp.
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|