TECHNET Archives

July 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 28 Jul 2015 17:26:52 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Mumtaz Bora <[log in to unmask]>
Message-ID:
Subject:
From:
Mumtaz Bora <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
<A285BD4A15094A5D989F88E4FDF8F211@MikePC>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (59 lines)
Hello Mike, Thank-you for your pointers regarding low melt solders. Much appreciated .

The soldering is using reflow oven, not hand soldering. The concern is some passives are not soldering very well and falling off the board with the SAC alloys, so one recommendation is to switch to low melt solders.


Thank-you
Mumtaz
858-795-0112
Peregrine  Semiconductor


-----Original Message-----
From: Mike Fenner [mailto:[log in to unmask]]
Sent: Sunday, July 26, 2015 8:44 AM
To: 'TechNet E-Mail Forum'; Mumtaz Bora
Subject: RE: [TN] Soldering NiPdAu finish components with low melt solder

Are you hand soldering or possibly have an oven with small number of zones?
I assume the driver here is difficulty of getting the joints to flow because of the heat sinking effect of the ground plain, and possible concerns for heat damage through prolonged heating times.
Low melting alloys such as SN/Bi [and its modified variants] may not improve matters. It's the tin that does the work in solder joint formation and in these low melting alloys it's relatively dilute so lower to work. In addition there is less energy due to the lower temperatures so the rate of joint formation is slow compared to eutectic and SAC types. If you then add NiPdAu to the mix that is decidedly not going to help. That stuff can be pretty close to wood in soldering terms.
Flux performance can be similarly impaired. If you are hand soldering by all means have a go, but you might find it is better to adjust tool performance so that you get a rapid rise to soldering temperatures before the heat sinking flattens you and/or to have some background heating to reduce the burden on local heating.
Don't forget that if choosing a lower MP alloy you are reducing the operating temperature range of your product and possibly reducing its life if it sees a lot of temperature cycling in service.

--
Regards

Mike Fenner
Bonding Services & Products
M: +44 [0] 7810 526 317
T: +44 [0] 1865 522 663
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mumtaz Bora
Sent: Thursday, July 23, 2015 3:46 PM
To: [log in to unmask]
Subject: [TN] Soldering NiPdAu finish components with low melt solder

Dear All, Good Morning,   Looking for some knowledge base  on soldering
NiPdAu finished components with low melt solder such as Sn42.0Bi57.6Ag0.4 to avoid wetting issues on a heavy copper plane board. Any insight and advise will be appreciated.

Thank-you
Mumtaz
858-795-0112
Peregrine  Semiconductor


CONFIDENTIALITY NOTE: The information transmitted, including attachments, is intended only for the person(s) or entity to which it is addressed and may contain confidential and/or privileged material. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and destroy any copies of this information.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


CONFIDENTIALITY NOTE: The information transmitted, including attachments, is intended only for the person(s) or entity to which it is addressed and may contain confidential and/or privileged material. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and destroy any copies of this information.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2