TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 2 Jul 2010 16:12:27 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Eric Christison <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="ISO-8859-15"; format=flowed
From:
Eric Christison <[log in to unmask]>
Parts/Attachments:
text/plain (52 lines)
I'm wondering about an issue we have with the dimensional stability of a
substrate made of FR4.

We're finding it's deforming during a flex attach operation, not by much
but enough to cause us a problem. We use ACF and a hot bar. The
substrate sees a temperature of 155 deg C for about 10 seconds. Someone
suggested that the movement may be due to incomplete curing of the
substrate.

I'm wondering if a temperature of 150 deg C for 10 seconds is likley to
have any effect at all on the matrix.

If it did, would the volume of the matrix increase, decrease or stay
much the same?

I realise that we'll see deformation due the application of pressure as
well but in some instances the substrate seems to be moving in the wrong
direction.

Thanks,

--
Eric Christison
Consumer&  Micro group
Imaging Division

STMicroelectronics (R&D) Ltd
33 Pinkhill
Edinburgh EH12 7BF
United Kingdom

Tel:	+44 (0)131 336 6165
Fax:	+ 44 (0)131 336 6001




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2