zinc is well known to have problem on corrosion and oxidation (on top of the
cat-whiskers David mentioned). I thought with all the reliability concern,
the shops like yours would stay far away from it due to the potential safety
issue. Unless you have unique application in mind (such as every thing in a
hermetic package under inert gas environment, for example).
http://www.reliability.com/articles/guest_article03.htm
my 2 cents.
jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of Charles Caswell
>Sent: Friday, August 30, 2002 4:53 PM
>To: [log in to unmask]
>Subject: Re: [TN] Zinc casting and solderability
>
>
>I haven't soldered zinc to a board but we have used cast zinc lugs
>that get wire soldered to them. We tin them first and I love the
>thin film it leaves on top of the solder pot.
>Charles Caswell
>
>-----Original Message-----
>From: David Douthit [mailto:[log in to unmask]]
>Sent: Friday, August 30, 2002 2:09 PM
>To: [log in to unmask]
>Subject: Re: [TN] Zinc casting and solderability
>
>
>Phil,
>
>Zinc will grow "whiskers" just like tin!
>
>David A. Douthit
>Manager
>LoCan LLC
>
>Phil Bavaro wrote:
>
>> Here is a question that I do not recall having come across ever before.
>>
>> A mechanical designer has posed the question of substituting
>zinc in place
>> of a copper as a raw material. This part will be required to be soldered
>> down to the circuit card it interfaces with as this is an RF assembly.
>>
>> Since Zinc alloys are very good for casting definition, is it
>also possible
>> to use Zinc as the base metal.
>>
>> Or does it require sealing with nickel and then tin plated in order to be
>> used for soldering applications?
>>
>> I realize that some of the new leadfree alloys contain low percentages of
>> zinc but this question is oriented towards high contents of zinc
>in the alloy.
>>
>> I will keep researching this topic but my first thoughts were that the
>> experts on this panel should be able to point me in the right
>direction at
>> least.
>>
>> Phillip A. Bavaro
>> QUALCO/\/\/\/\ Incorporated
>> CCA Technical Support
>> Engineer, Senior
>> [log in to unmask]
>> Pager (858) 271-3640
>> Tel (858) 658-2542 Voice mail
>> Cell (858) 682-6434 (offsite, after hours)
>> Fax (858) 658-1584
>>
>>
>-------------------------------------------------------------------
>--------------
>> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send
>e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|