I would like to draw on the experience of others who have may have used an
OSP coating with an aqueous wash process.
The material is Entek Plus CU-106A and was specified for boards intended for
a no-clean process. The board will sees two passes thru a surface mount line
plus some hand soldering of thru-hole parts.
My questions:
1. Is this coating compatible with a water soluble flux (Alpha WS609 paste)
process with cleaning in 130 degree F DI water (in-line cleaner, no
chemistry). Keep in mind it will go thru the cleaner at least three times
(two surface mount and one thru-hole pass.)
2. Is OSP in general compatible with aqueous cleaning or is it primarily
designed for a no-clean process?
Thanks in advance for all help.
=========================
Bob Barr
Manufacturing Engineering
Formation, Inc.
=========================
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|