TECHNET Archives

February 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 12 Feb 2008 18:06:37 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Igoshev, Vladimir" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset=utf-8
From:
"Igoshev, Vladimir" <[log in to unmask]>
Parts/Attachments:
text/plain (1 lines)
That is what I had thought when I send my first e-mail. Then I saw the pictures and the Ni layer looked normal relatively to the thickness of Cu. As I've said before, I'm always confused with microinches :-), but now it looks I'm not alone, which makes me feel better :-)



Vladimir



----- Original Message -----

From: Stadem, Richard D. <[log in to unmask]>

To: TechNet E-Mail Forum <[log in to unmask]>; Igoshev, Vladimir

Sent: Tue Feb 12 17:44:42 2008

Subject: RE: [TN] Through Hole Pad Solder Non-Wetting



No, it is not. Standard ENIG is optimally 150 uinches of nickel, with between 3-6 uinches of gold over it, per the IPC spec. What Paymon has is not ENIG.



Electroless Nickel Thickness APPENDIX 4 3.2.1 

3 to 6 μm

[118.1 to 236.2 μin]

Immersion Gold Thickness APPENDIX 4 0 

0.05 μm minimum

[1.97 μin minimum]



Paymon, if you in fact have only 1-3 uinches of nickel, you are really screwed.

Even if you have 1-3 um of nickel, you are under the minimum of 3 um.

This will cause the copper to leach through the nickel and react with the gold, and cause all kinds of solderability issues.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Igoshev, Vladimir

Sent: Tuesday, February 12, 2008 2:41 PM

To: [log in to unmask]

Subject: Re: [TN] Through Hole Pad Solder Non-Wetting



Sorry, I'm always confused with microinches and microns. :-( The thickness is fine.



Vladimir



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Paymon Sani

Sent: Tuesday, February 12, 2008 2:30 PM

To: [log in to unmask]

Subject: [TN] Through Hole Pad Solder Non-Wetting



Hello All,



 



We experienced solder non-wetting to a PCB through-hole component pad surface. The PCB surface finish is ENIG. The microsection results from the suspect PCBs show that the Nickel plating is thin from 1 to 3 micro-inches. We related the thin Nickel plating to Nickel corrosion and PCB surface non-wetting. However, the microsection also revealed copper corrosion at Copper to Nickel interface! I have never seen the copper corrosion in the past and I would like to ask if any of you has a similar experience in the past. What could be the cause of copper corrosion? I have few images if you are interested to see them.



 



Regards,



Paymon





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------






ATOM RSS1 RSS2