Hi Leif,
A few quick thoughts
Conformal coating provides a water resistant barrier, is quick, cost effective
and easy. Conformal coating can be applied over entire assembly or applied
selectively.
Underfill will also help with CTE mismatch and is a slow production process
(possibly warranting multiple machines to meet thru-put needs).
When considering routes for moisture absorption, humidity migration thru the
circuit board material (BT Resin or FR4) will be minimized by the solder resist.
That said, anyone who has baked a board to measure dry weight has seen the
measurable amount of absorbed moisture present in an assembly.
Both processes are benefited and in many cases require a pre-clean step to
promote adhesion, flow, and minimize entrapped contaminants (including
corrosive elements).
Rework can be a bear with both.
Cordially,
Shean Dalton
FHP
512.971.2850
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|