TECHNET Archives

October 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Ioan TEMPEA <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan TEMPEA <[log in to unmask]>
Date:
Fri, 10 Oct 2014 12:34:48 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (77 lines)
Mike,

I fully understand the futile debate if I wanted to validate the supplier's measurements.

What about using the viscometer for lot to lot consistency assessment, i.e. I set the baseline to a known good lot and then simply measure the lot to lot variation? Is a viscometer the proper tool for this?

Thanks,

Ioan Tempea, P. Eng.
Manufacturing Engineer, Satellite Systems 

MacDonald, Dettwiler and Associates Corporation, 21025 Trans-Canada Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2
Tel: +1-514-457-2150 x3556
www.mdacorporation.com

This e-mail, and any attachments, are intended solely for the use of the intended recipient(s) and may contain legally privileged, proprietary and/or confidential information. Any use, disclosure, dissemination, distribution or copying of this e-mail and any attachments for any purposes that have not been specifically authorized by the sender is strictly prohibited. If you are not the intended recipient, please immediately notify the sender by reply e-mail and permanently delete all copies and attachments. This email is for informational purposes only and shall not be interpreted to authorize or conclude a binding agreement between MDA and any other party unless this email contains or is accompanied by an express written confirmation of MDA's intention to enter into a binding agreement, such confirmation shall only be provided by an authorized representative of MDA.


-----Message d'origine-----
De : Mike Fenner [mailto:[log in to unmask]] 
Envoyé : Friday, October 10, 2014 8:27 AM
À : 'TechNet E-Mail Forum'; Ioan TEMPEA
Objet : RE: [TN] Viscometer

Testing for what?
If you are considering it for goods inwards testing or verifying aged material, then I would urge you to consider other ways. (Print test or extrusion rate or similar.) Unless you can exactly duplicate supplier test conditions (and even then) you are probably in for a world of pain. It is likely your numbers will differ from theirs.  This will give you endless debates back and forth on the meaning of the numbers and possibly needless rejections and resulting "discussions".

If you do go ahead with that then as other 'netters have said you will need the same kit (implicit in above) as your material vendors. Depending on the other materials you wish to investigate you may require more than one type of viscometer. Which ever way you go I would suggest you use your number as an index only not an absolute measurement. You will also need to ask for actual viscosity of each batch to be supplied on C of C (if not now) as some people certify product to be as specified wchich will only mean within range, to get any meaningful data.
Having said that, if you did had the actual viscoity as supplied you would not need to do your own as you would have a measurement you could rely on and do SPC like things with it. 

If you just want to explore rheology the classic Brookfield is really an obsolete method as it doesn't really measure rheology. Those people who give Brookfield data do so only for historical or continuity reasons. There are much better systems, which are faster and less condition of test dependent.
The other problem you could have is sample size, some systems can require a test sample larger than you might have [or can afford if looking at conductives.] 

Hope this helps.


Regards 
 
Mike 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan TEMPEA
Sent: Thursday, October 09, 2014 1:08 PM
To: [log in to unmask]
Subject: [TN] Viscometer

Dear Technos,

I need to buy a viscometer, what are your suggestions?

The main usage will be testing conductive epoxies, but might be used for other materials too.

Thanks,

Ioan Tempea, P. Eng.
Manufacturing Engineer, Satellite Systems

[cid:[log in to unmask]]

MacDonald, Dettwiler and Associates Corporation, 21025 Trans-Canada Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2
Tel: +1-514-457-2150 x3556
www.mdacorporation.com<http://www.mdacorporation.com/>

This e-mail, and any attachments, are intended solely for the use of the intended recipient(s) and may contain legally privileged, proprietary and/or confidential information. Any use, disclosure, dissemination, distribution or copying of this e-mail and any attachments for any purposes that have not been specifically authorized by the sender is strictly prohibited. If you are not the intended recipient, please immediately notify the sender by reply e-mail and permanently delete all copies and attachments. This email is for informational purposes only and shall not be interpreted to authorize or conclude a binding agreement between MDA and any other party unless this email contains or is accompanied by an express written confirmation of MDA's intention to enter into a binding agreement, such confirmation shall only be provided by an authorized representative of MDA.


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2