TECHNET Archives

May 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 4 May 2016 13:14:20 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Stadem, Richard D." <[log in to unmask]>
Parts/Attachments:
text/plain (16 lines)
In looking at the test methods for a proprietary semi-solder paste/solder ink, I wanted to test slumping. The material I am qualifying is actually a blend. I have the small staggered stencil, but  J-STD-005  says:


3.7 Solder Ball Test; the solder paste when tested in accordance with 3.7.1 shall meet the requirements specified.

3.7.1 Type 1-6 Powder; the solder paste with Type 1 through 4 type powders defined in IPC-TM-650, Test Method 2.4.43, shall meet the acceptance criteria presented in Figure 3-3.

3.7.2 Type 7 Powder; the solder paste with type 7 powders does not require testing and should be determined AABUS.

So how do I test a Type 5 or 6? Is Method 2.4.43 applicable?

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 