TECHNET Archives

June 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 23 Jun 2009 12:54:03 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Kenneth Wood <[log in to unmask]>
Subject:
From:
Kenneth Wood <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (117 lines)
I think they are just sweating from the high speed data running through
them...

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: Tuesday, June 23, 2009 9:05 AM
To: [log in to unmask]
Subject: Re: [TN] "Blumpie" looking connector leads...

It's not dewetting of solder, more like a blistering/bubbling of the lead
finish. Try just heating a connector on its own and I suspect you will
generate the problem.
Blumpie is a great word BTW.

Regards
 
 
Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, June 23, 2009 12:49 PM
To: [log in to unmask]
Subject: [TN] "Blumpie" looking connector leads...

 Morning all!
 
Trying to stay cool here! Broke 100 degrees yesterday and Sunday, and
it's probably going to break 100 degrees today. Summer has come with a
vengeance! 
 
Ran across something yesterday that I've never seen before. We build a
board that uses this AMP Densipac SMT connector:
 
http://tinyurl.com/nqbpcp
 
 
We've built a lot of these boards before without any issues at all. This
latest run we have something going on with these particular connectors.
Here's a photo of them on the PCB:
 
http://stevezeva.homestead.com/files/AMP_Connectors.jpg
 
You can probably see that the leads have this "Blumpie" look to
them...both bumpy and lumpy. This is fresh out of the reflow oven.
Here's a closer look:
 
http://stevezeva.homestead.com/files/Connector_Blumpies.jpg
 
If you notice the two pins either side of the white line look fine. They
are the anchor pins that are for mechanical strength for the
connector...they are not I/O pins. The rest of the board looks
absolutely fine too. Not a bit of problem. It's just the I/O pins. We
have noticed that connectors with certain date codes don't have this
problem. Also, before reflow the connectors look okay. Luckily we've
only built a few boards, and we're stopping until we can get to the
bottom of this...
 
Have any of you ever seen "blumpie" connectors like these before?
 
Steve

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended
solely for the addressee(s) and may be legally privileged and/or
confidential. If you are not the intended recipient, please contact the
sender by return and delete the material from any computer. Any review,
retransmission, dissemination, or other use of, or taking of any action in
reliance upon this information by persons or entities other than the
intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and
unauthorized alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Indium Corporation
makes no warranty as to accuracy or completeness. Indium Corporation does
not accept responsibility for changes made to this email after is was sent.
Any opinions or recommendations expressed herein are solely those of the
author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2