KennyB,
This one just went around within the last two weeks. Typical FR-4 contains neither of these chemicals. FR-4 flame retardant is TBBPA. Tetrabromo Bisphenol-A
Best regards,
Dave
David W. Bergman, CAE
Vice President Standards, Technology and International Relations,
IPC
2215 Sanders Road #250
Northbrook, IL 60062-6135
Dir. Line 847-790-5340 Main 847-509-9700
Mobile 847-867-1388
Dir. Fax 847- 504-2340 Main Fax 847-509-9798
E-mail [log in to unmask] web www.ipc.org
-----Original Message-----
From: Bloomquist, Ken [mailto:[log in to unmask]]
Sent: Thursday, June 10, 2004 8:39 AM
To: [log in to unmask]
Subject: [TN] A Bromine/EU Question
Good morning Technetters,
One of our customers has asked the following question:
**********************************************************
As you already probably know, the European Directive 2003/11/CE of the 6th of February 2003 will be applicable in Germany on the 30th of June 2004 and within the whole European Union as from the 15th of August 2004.
This Directive aims at banning the marketing and use, within the European Union, of the following hazardous substances when accounting for more than 0.1% of the total weight of the product and/or any part thereof:
- PENTABROMODIPHENYL ETHER (CAS N° 32534-81-9)
- OCTABROMODIPHENYL ETHER (CAS N° 32536-52-0)
These substances are currently used as fire retardants to provide appropriate fire resistance and self extinguishing properties to the products in which they are incorporated.
**********************************************************
I have two questions for you chemical guys;
1. Does typical FR4 laminate contain these chemicals in the amount they talk about?
2. What the heck do they mean by "total weight of the product and/or any part thereof"? What do they consider a "part thereof"? (subassembly, component, bare board)?
Thanks in advance for any information provided.
KennyB
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|