TECHNET Archives

April 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dwight Mattix <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 1 Apr 2004 09:37:28 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (72 lines)
Werner's comments are on target (as usual).  As we used to say about an
avionics tech I worked with in the Navy, "He's not always right but you
have to ask yourself, 'How often is he wrong?'"  :-)

Werner gave a good summary of obvious/likely causes to consider first
off.  One other factor we've encountered that you may want to keep in mind
is holewall quality.  Specifially, itsy bitsy pinholes in the plating as
the result of small localized plating voids -- typically at the ends
of  glass fibers protruding into the hole (nodules, skip plating, plating
folds, et al).  So while you're looking at cross sections and focusing on
the solder/component lead don't forget to look at the pwb hole wall/plating
as well.


cheers,

Dwight Mattix
Sr Staff Quality Engineer
Corporate Engineering, Qualcomm, Inc

At 02:11 PM 3/31/2004 -0500, Morse, Carrie wrote:
>We recently had circuit card assembly sent out for cross sectioning.
>One of the leads for a thru-hole device has voids -- perfectly round
>voids.  The component body prevents us from seeing the top of the solder
>joint (which, if we could have seen, we would have seen a void).  The
>bottomside of the joint has a void, but, would not have been visible
>without cross sectioning.  The board was sent out for cross sectioning
>to evaluate a different problem, but, cross sectioning was done on a
>sample basis to evaluate the entire board.  In other words, this
>specific component has not been a problem (yet).
>
>My questions are as follows:
>1.  What causes the voids over the wave?  My first guess is insufficient
>preheat or dwell time.  My second guess is materials (moisture in the
>board).  Are these valid root causes?  What else should I consider?
>2.  Are the voids detrimental to the reliability of the board?  We use
>OA flux.  I bet there is flux entrapped.  That can't be good.
>3.  What is the acceptance criteria for voids in Thru-Hole parts?
>IPC-A-610 sec 6 covers circumferential wetting as well as percent fill
>as these are visible without cross sectioning.  Is there a spec that
>covers what a thru-hole solder joint should look like cross sectioned?
>
>TIA,
>Carrie
>
>
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2