Jeffrey - the new ENIG spec IPC 4552 recommends the minimum Au to be 2
microinches at -4 standard deviation from the mean (typical value being 3 to
5 ) and for nickel to be 120 to 240 microinches. There is no recommendations
based on part type.

Gerard O'Brien
co-chairman 4552 committee
Photocircuits corp.

-----Original Message-----
From: McGlaughlin, Jeffrey A [mailto:[log in to unmask]]
Sent: Friday, December 06, 2002 10:54 AM
To: [log in to unmask]
Subject: [TN] ENIG FINISH SPEC'S


What are the standard finish thickness for Electroless Nickel/Immersion Gold
for fine pitch (0.75mm) BGA boards?

Jeffrey A. McGlaughlin CID
Sr. Designer
Battelle Memorial Institute
Columbus Ohio
[log in to unmask]

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2